affiliation not provided to SSRN
Mg-Bi-Ca-Zn alloy, hot extrusion, bimodal grain structure, grain boundary reinforcement, dislocation strengthening
magnesium alloy, Microstructure, texture, Damage behaviors
7003 aluminum alloy, High-speed impact, mechanical response, Microstructure evolution, Adiabatic temperature rise
L12-precipitate, First-principles calculations, Partial least squares regression, Competitive mechanism
AZ31 magnesium alloy, Square extrusion, Heat Treatment, Microstructural evolution, Crush energy absorption